For a prototype, I put H7/p6 on a drawing far less often than people expect. On a 10 mm pin it gives anywhere from zero to 24 micrometres of interference, which means one assembly may push together by hand and the next needs an arbor press and won't come apart without damage. If the part is going to be opened, adjusted or re-machined (and prototypes always are), a slip fit plus something else to hold it is usually the better call.
Press fits have their place, and it's a small one.
What H7/p6 means in micrometres
The letters hide the numbers, so here they are for a nominal 10 mm diameter. An H7 hole may be anywhere from 10.000 to 10.015 mm. A p6 shaft may be anywhere from 10.015 to 10.024 mm. Put the biggest hole on the smallest shaft and you have zero interference, a line-to-line fit. Put the smallest hole on the biggest shaft and you have 24 µm.
That's the whole story of H7/p6: it's classed as an interference fit, but the loose end of the band isn't holding anything.
| Fit at Ø10 | Shaft limits (µm) | Result | How it assembles |
|---|---|---|---|
| H7/g6 | −5 / −14 | 5 to 29 clearance | Slides freely, slight play |
| H7/h6 | 0 / −9 | 0 to 24 clearance | Pushes in by hand, locates well |
| H7/k6 | +10 / +1 | 14 clearance to 10 interference | Light tap with a mallet |
| H7/m6 | +15 / +6 | 9 clearance to 15 interference | Mallet or light press |
| H7/p6 | +24 / +15 | 0 to 24 interference | Press, semi-permanent |
| H7/s6 | +32 / +23 | 8 to 32 interference | Press or shrink, permanent |
These values belong to the 6 to 10 mm size band of ISO 286. They grow with diameter: for sizes over 10 and up to 18 mm the H7 hole opens to +18 µm and p6 becomes +29 / +18. Always look up the band for your actual diameter, because a fit copied from a 10 mm pin onto a 40 mm bush is a different animal.
Why press fits bite on prototypes
In production, a few thousand parts spread themselves across the tolerance band and the average assembly sits comfortably in the middle.
You're making three.
Each pair lands wherever it lands inside that 0 to 24 µm window, and you find out at the bench.
Then there's the hole itself. A drilled hole isn't H7. Getting there needs a reamer or a boring pass, the shop needs the right reamer in the drawer, and a hand-fed reamer in a blind aluminium hole can easily cut 10 µm oversize. Now your press fit is a slip fit and nobody knows until the pin falls out. If a fit matters, I ask the shop for measured values on those diameters, not a general inspection tick.
Shafts are the same problem from the other side. Turning a one-off pin to p6 means holding a 9 µm band on a lathe, which costs money. Ground dowel pins come off the shelf at m6 for a few cents each, so it's nearly always cheaper to design around a bought pin than to specify your own shaft tolerance.
And prototypes come apart. Press a hardened steel pin out of a 6061 housing and it scores the bore on the way, so the second assembly is looser than the first and the third is a guess.
A founder sent me a small gearbox housing last year with H7/p6 called out on all eight pins and on both bearing seats. The machine shop had priced reaming and inspection on every bore, and on the first assembly a pin went in dry and slightly crooked and cracked a thin boss. We changed six of the eight pins to H7/h6 with retaining compound, kept press fits on the two locating dowels, and the second housing went together on a bench in about twenty minutes.
Nothing about the design got worse.
Temperature quietly eats your interference
This is the part people get wrong most often. Aluminium expands at about 23 µm per metre per kelvin, steel at about 12. Put a steel pin in an aluminium housing and warm the assembly up, and the hole grows faster than the pin.
The sum is short. For a 10 mm pin and a housing running 60 K above the temperature it was assembled at (a motor mount at 80 °C, say), the difference is 11 × 10-6 × 10 mm × 60, which is 6.6 µm. A fit that started with 5 µm of interference is now loose. At 50 mm diameter the same temperature rise gives 33 µm, and that swallows most of the H7/p6 range at that size, which runs from 1 to 42 µm. So does a press fit in aluminium hold at temperature? Only if you've checked the cold minimum against the hot growth.
The same physics is useful in the other direction. Heat that aluminium housing from 20 to 150 °C and a 10 mm bore grows by about 30 µm, more than the worst-case 24 µm interference, so the pin drops in under its own weight and locks as the housing cools. A shrink fit like that doesn't score the bore, and for anything permanent I prefer it to pressing.
Printed and plastic parts ignore ISO fits
I see H7 on drawings for FDM-printed brackets fairly regularly. It means nothing there. The tolerance band is 15 µm wide and the process spread on a printed hole is 100 µm or more, with holes typically coming out 0.1 to 0.2 mm undersize and varying with print orientation.
What works is a test coupon. Print a small block with seven holes stepping in 0.05 mm increments, from 0.1 mm under nominal to 0.2 mm over, in the same material and the same orientation as the real part. Try the actual pin in each. It's twenty minutes of printing and it tells you more than any table. Powder-bed processes are tighter and more repeatable, but still nowhere near reamed-hole accuracy.
Plastics also creep. A pin pressed into ABS or PETG feels solid on day one and relaxes over the following weeks, faster if it's warm. For printed and moulded functional prototypes I use heat-set brass inserts, a clamping feature with a screw, or a snap, and I keep interference fits for metal.
What I'd actually put on the drawing
It comes down to whether the joint ever has to come apart, and to what's holding the load.
- Needs to come apart or be adjusted: H7/h6 or H7/g6, retained by a set screw on a flat, a clamp, or retaining compound.
- Locating dowels between two plates: standard m6 dowel pins, H7 in the plate that keeps the pins, and F7 (+13 / +28 µm at 10 mm) in the plate that lifts off, so it slips on without a fight.
- Permanent pin or bush in metal: H7/p6 is fine, with a 15 to 30 degree lead-in chamfer about 0.5 mm long, a drop of oil, and an arbor press pushing square. Never a hammer.
- Bearings: use the bearing manufacturer's fit table for your load case, not a general rule from me or anyone else.
Blind holes need a vent. A pin pressed into a sealed bore compresses the air underneath and either stops short or creeps back out overnight, so I add a small flat along the pin or a 1 mm cross hole.
On the drawing itself, I write the limits in brackets after the fit code: Ø10 H7 (+0.015 / 0). Not every small shop has the ISO 286 tables open, and it removes any argument about which size band applies. I also call out Ra 1.6 or better on both surfaces, because on a rough bore the peaks flatten during pressing and take a few micrometres of effective interference with them. The general tolerance block won't cover any of this, which I went through in the piece on ISO 2768 and when to override it, and the rest of what belongs on the sheet is in the manufacturing drawing checklist.
I used to work with 5 µm assembly tolerances on CNC parts for microfluidics. The lesson that stuck is that a tolerance you can't measure in the shop that makes the part is a wish, not a specification.
If you've got a housing with fits on it and you're not sure which ones deserve to be tight, that's a good subject for a first look. You can request a free initial DFM review of one part or assembly and I'll send back short written observations, fits included. If the design is still moving, mechanical design and 3D modeling is where I'd start instead.