For most injection moulded parts, the practical minimum wall thickness sits between about 0.6 and 1.2 mm depending on the material, and the comfortable range for a part that fills easily is 1.5 to 3 mm. Polypropylene and nylon will fill walls under 1 mm. Polycarbonate and ABS start to struggle below 1 mm on anything bigger than a small clip. But the material is only half the answer. The other half is how far the plastic has to flow through that wall, and that's the number most drawings never mention.
Typical wall thickness ranges by material
These are the starting ranges I use at concept stage, before a moulder has seen the part. They line up with what most moulders and published design guides recommend, rounded to numbers I can actually remember:
| Material | Practical minimum (mm) | Comfortable range (mm) |
|---|---|---|
| PP (polypropylene) | 0.6 | 0.8 to 3.8 |
| PE (HDPE, LDPE) | 0.8 | 0.8 to 3.0 |
| PA6 / PA66 (nylon) | 0.5 | 0.8 to 3.0 |
| POM (acetal) | 0.8 | 0.8 to 3.0 |
| ABS | 1.0 | 1.2 to 3.5 |
| PC/ABS | 1.0 | 1.2 to 3.5 |
| PC (polycarbonate) | 1.0 | 1.2 to 3.8 |
| PMMA (acrylic) | 0.8 | 1.0 to 3.8 |
| TPE / TPU overmould | 0.5 | 0.8 to 3.0 |
Glass-filled grades shift everything upwards. A 30% glass-filled nylon flows worse than unfilled nylon and wears thin sections of the tool, so I'd add 0.3 to 0.5 mm to the minimum.
Treat the minimum column as a warning line, not a target.
Flow length matters more than the table
A 0.8 mm wall in ABS is easy on a 20 mm clip and nearly impossible on a 200 mm lid. The plastic starts freezing against the cold steel the moment it enters the cavity, so a thin, long wall either short-shots or needs so much pressure that the tool flashes.
The quick check is the flow length to wall thickness ratio, measured from the gate to the furthest point of the part. Rough limits I work with: PP and PE can go up to around 250:1, nylon around 200:1, ABS 150 to 200:1, and PC closer to 100 to 150:1 because it's so viscous. A PC housing with 1.2 mm walls is therefore comfortable up to about 150 mm of flow. Past that, you either thicken the wall, add a gate or move the gate to the middle.
The ratio is also why gate position belongs in a DFM discussion from the start. The same part can be fine with a centre gate and unmouldable with an edge gate.
Thinner isn't automatically cheaper
This is the counter-intuitive part for most founders. They thin the walls to save plastic, and the plastic was never the expensive bit.
On a small housing weighing 40 g, going from 2.0 to 1.5 mm might save 10 g of ABS per part. At typical resin prices that's a fraction of a cent. Meanwhile, the thinner wall needs higher injection pressure, which can push the job onto a bigger press, and it tightens the process window so the moulder scraps more parts at startup. In bad cases it forces a hot runner or a second gate, and that's a real tooling cost in the thousands of euros.
Going thicker has its own price. Cooling time grows roughly with the square of wall thickness, so a 3 mm wall cools about 2.25 times longer than a 2 mm one, and cycle time is what you pay for on every single part. Thick walls also sink and hide voids. So the target is the thinnest wall that fills comfortably, not the thinnest wall that fills at all.
Keep it uniform, then add ribs
Uniformity beats any specific number. Plastic shrinks as it cools, and a section that's 3 mm next to one that's 1.5 mm shrinks by different amounts, which gives you warpage, sink marks over the thick zone and residual stress that shows up later as cracks around screws.
The rules I check on every part:
- Keep wall variation within about 10 to 15% across the part where you can.
- Where thickness must change, blend it with a gradual transition, around three times the thickness difference in length, never a step.
- Ribs at 50 to 60% of the wall they stand on (closer to 40% for glossy surfaces where sink marks show), with 0.5 to 1 degree of draft per side.
- Core out bosses and thick lugs rather than leaving solid blocks.
If you need stiffness, ribs are almost always better than more wall. A 1.8 mm wall with a few ribs is stiffer and cools faster than a 3 mm plain wall.
A housing that came back short
A couple of years ago I reviewed a handheld device housing for a small startup: PC, 1.2 mm nominal wall, about 165 mm long, gated at one end because that's where the cosmetic face wasn't. On paper every wall met the "PC minimum 1 mm" line from a design guide. The first T1 shots didn't fill the far corner, and the moulder pushed pressure until the parting line started flashing.
Nothing was wrong with the wall in isolation. The flow ratio was close to 140:1 at the far corner, plus a row of thin snap features right at the end of fill. We went to 1.6 mm on the main shell, kept 1.2 mm on the snaps, and the T2 parts filled without drama. The tool change cost less than another round of pressure tuning would have.
What I'd actually do on a new part
Start at 2 mm for ABS, PC and PC/ABS, and 1.5 mm for PP and nylon, then only go thinner where there's a reason: weight, a tight envelope, a living hinge. Check the flow ratio from the planned gate before you get attached to a number. Run a quick fill analysis if the ratio is anywhere near the limits above. Then ask the moulder. They know their presses and their material lots better than any table, mine included.
I'd also put the nominal wall on the drawing as a note, with which features are allowed to deviate. It saves a round of questions at quoting. The manufacturing drawing checklist covers what else should be on there.
Wall thickness is one of the first things we look at in an injection molding DFM review, along with draft, gate position and undercuts. If you're still at the concept stage, the injection molding DFM questions page lists what a moulder will ask, and the wider DFM review service covers machined and sheet metal parts too. If you have a part you're unsure about, you can request a free initial DFM review of one part and get written observations on the walls before anyone cuts steel.