Rib Thickness Ratios and Where Ribs Go Wrong

The short version: make a rib 50 to 60% of the wall it stands on, no taller than about three times that wall, with 0.5 to 1 degree of draft per side and a small radius at the base. Drop to 40% on glossy or high-shrink parts. Most rib problems I see in reviews aren't ratio problems, though. They're ribs in the wrong place, ribs that meet in a lump, or ribs the tool can't properly cut and fill.

Here are the numbers, then the ways they go wrong.

The ratios, in one table

Everything is expressed against the nominal wall, T. For a typical 2.5 mm ABS housing wall, that gives a 1.25 to 1.5 mm rib up to 7.5 mm tall.

FeatureGuidelineExample at T = 2.5 mm
Rib thickness at base0.5 to 0.6 T (0.4 T for gloss, PP, PA)1.0 to 1.5 mm
Rib heightup to 3 T7.5 mm
Draft per side0.5 to 1.5 degreesabout 0.13 mm per side at 1 degree over 7.5 mm
Base radius0.25 to 0.5 T0.6 to 1.25 mm
Spacing between ribsat least 2 T5 mm or more
Boss wall thicknessabout 0.6 T1.5 mm

None of these are laws. They come from resin suppliers' design guides and decades of moulders getting burned, and different sources disagree by ten percent here and there. Treat them as where to start, then talk to whoever cuts the steel.

Why the rib has to be thinner than the wall

Plastic shrinks as it cools, and thick sections cool last. Where a rib meets a wall, the junction is thicker than either, so the core of that junction is still molten after the surfaces have frozen. As it shrinks it pulls the outer skin inwards. That's the sink mark on the cosmetic face, directly opposite the rib.

You can check this in CAD in under a minute. Draw the inscribed circle at the rib base in a section sketch. With a 2.5 mm wall, a 1.5 mm rib and a 0.6 mm radius, the circle comes out near 3 mm, roughly 20% over nominal. That's usually survivable under a texture. Make the rib the full 2.5 mm and the circle grows to about 3.4 mm, nearly 40% over. That sinks in almost any resin.

The same sketch shows why big fillets backfire. A generous base radius feels like good practice (less stress concentration, better flow), and it is, up to a point. But every extra tenth of radius adds mass to the junction. I keep it at 0.25 T on cosmetic parts and go towards 0.5 T only where the rib is structural and the outside face is hidden or textured.

Height, draft and the thin top

This is the bit people forget to work out. A rib that's 1.5 mm at the base with 1 degree of draft per side loses about 0.035 mm of thickness for every millimetre of height. At 7.5 mm tall the tip is about 1.24 mm. Fine. Stretch that same rib to 20 mm because you wanted more stiffness, and the tip is down to 0.8 mm. Now it's hard to fill, it traps gas and burns, and it grips the steel on ejection.

From the toolmaker's side, a deep thin rib is a deep thin slot. It's usually cut by EDM, it's hard to polish, and it's hard to vent. Poor polish in a deep slot means the part hangs on ejection, and you get drag marks or stress whitening at the rib root. Making the rib fatter instead just brings the sink back.

What do you do when one rib isn't stiff enough? Add a second one.

Two ribs of 3 T at a spacing of 2 to 3 T beat one rib of 6 T for mouldability every time. Bending stiffness goes with the cube of height, so there's a real penalty for staying short, but you usually have room to pay it in rib count.

Where ribs go wrong in real parts

The ratio table gets most of the attention. These are the things I mark up far more often.

  • Rib crossings. Two 1.5 mm ribs crossing at ninety degrees make a junction with a diagonal over 2 mm, sitting on a wall, with fillets. It's a hot spot. Core it out with a small pin or offset the ribs into a T.
  • Ribs running into bosses and corners. A rib that ties a boss to the side wall is good practice. Three ribs and a boss merging 2 mm from an outside corner is a lump.
  • Ribs against the flow. A long rib perpendicular to the fill direction can hesitate, with the melt racing past along the wall and filling the rib late. Short shots and weld lines at the rib tip follow.
  • Ribs blocking the tool. A rib that isn't parallel to the pull direction is an undercut. I see this on angled internal walls more often than you'd think.
  • Ribs with no job. Added "for stiffness" with no load path. They add cycle time and sink risk and stiffen nothing.

A founder brought me a handheld housing a couple of years back with a visible line across the display bezel in every first-shot sample. The moulder had already tried more pack pressure. The cause was a single stiffening rib under the bezel drawn at full wall thickness, 2.2 mm on a 2.2 mm wall, because the designer had extruded it from the wall sketch. We thinned it to 1.1 mm and split it into two, and the mark dropped to something a light texture covered.

Thinning a rib means putting steel back into the slot, which is the expensive direction. The tool needed a small insert and they lost two weeks. In CAD it would've been a ten-minute edit, and it's the reason I start ribs thin: making one thicker later only means cutting a little more steel away.

Bosses follow the same logic

A screw boss is a rib bent into a circle, and it sinks for the same reason. Keep its wall near 0.6 T, don't let it touch the side wall directly (stand it off and connect it with a rib of the usual thickness), and core the hole deep enough that the material under the boss isn't thicker than nominal. Gussets on a tall boss follow rib rules too: 0.5 T thick, with draft.

The trade-off is strength. A boss thin enough not to sink may be too thin for the hoop stress from a thread-forming screw, and that's a real conflict, not something a ratio resolves. When it bites, I'd sooner hide the sink (texture, a local recess, a label area) than crack a boss in the field. I went through the screw-side numbers separately in the piece on screw boss design.

Does the material change the numbers?

Yes, quite a lot. Amorphous resins such as ABS, PC and PC/ABS shrink around 0.5 to 0.7% and tolerate ribs at 0.6 T, sometimes a little more under texture. Semi-crystalline ones (PP, PA, POM) shrink two to four times as much, so 0.4 to 0.5 T is safer. Glass-filled grades shrink less overall but they warp, because the fibres line up with the flow and the part shrinks differently along and across them. With 30% glass, rib direction starts to decide which way the part bows.

Surface finish shifts it again. High-gloss black shows a sink only a few hundredths of a millimetre deep. A medium texture hides several times that.

What I'd actually do on a new housing

Set the nominal wall first and write it down. Then make rib thickness a parameter tied to it (0.55 times the wall, one user parameter in Fusion 360), so nobody extrudes a rib from the wrong sketch at 11 pm. Draft the ribs when you create them, not at the end, because adding draft later is when tips go to 0.6 mm unnoticed.

Before release, cut three or four sections through the worst-looking junctions and measure the inscribed circles. Anything more than about 25% over nominal gets cored or thinned. It's crude, it takes fifteen minutes, and it catches most of what a moulder would send back. The rest of my pre-release list is in the DFM checklist, and the things worth asking a moulder directly are collected under injection molding DFM questions.

If you'd like a second pair of eyes on a ribbed part before it goes out for quotes, that's what a DFM review is for. The first one, for a single part or assembly, is free: you can request a free initial DFM review and I'll send back short written observations, ribs included.

Questions people ask

How thick should a rib be in an injection molded part?

Start at 50 to 60% of the nominal wall for amorphous resins such as ABS or PC, and 40 to 50% for PP, PA and POM or for any high-gloss cosmetic face. Measure it at the base, before draft, and check the junction with an inscribed circle in a section view.

How tall can a rib be?

About three times the nominal wall is the usual limit. Taller ribs get thin at the tip once draft is applied, which makes them hard to fill, vent and eject. If you need more stiffness, add a second rib at a spacing of at least twice the wall instead of going higher.

Do ribs need draft?

Yes. Use 0.5 to 1.5 degrees per side, with 1 degree as a comfortable default. Ribs sit in deep, narrow slots in the tool that are difficult to polish, so without draft the part drags on ejection and can whiten or tear at the rib root.

Can I fix a sink mark from a rib without changing the tool?

Sometimes it can be reduced with higher pack pressure, longer hold time or a lower melt temperature, but processing rarely removes it fully. Lasting fixes are geometric: thin the rib, core the junction or add texture to the outside face. Thinning requires adding steel, so it's far cheaper to get right in CAD.

Want a second pair of eyes on your part?

The first DFM review of one part or assembly is free: short written manufacturability notes, no simulation, no redesign. We sign an NDA first if the CAD is confidential.

Request a free initial review

More from the blog