Sink Marks: Why They Appear and the Design Fixes That Work

Sink marks in injection molding come from one thing: a thick section of plastic keeps cooling and shrinking after the skin around it has frozen, so it pulls the surface inward. The usual causes are ribs or bosses that are too thick where they meet the wall, local thick spots, and too little packing pressure or time. The design fixes work better than the process ones, and they're far cheaper to make before the steel is cut.

I find sink risk in almost every first design review of a plastic part, so here's how I spot it and what I change.

What's physically happening under the dimple

Plastic shrinks as it cools. Amorphous materials like ABS and PC typically shrink around 0.4 to 0.7%, semi-crystalline ones like PP and PA6 more like 1 to 2.5%, depending on grade and filler. That's fine when the wall is uniform, because the whole part shrinks together and the tool is cut to compensate. Uniform shrinkage is predictable. Local shrinkage isn't.

The trouble starts at intersections. Where a 1.2 mm rib meets a 2 mm wall, the material at the root is effectively thicker than either, often 30 to 40% thicker once you add the root fillet. The outer skin freezes against the cold steel within a second or two, while the core at that root is still molten, and as it shrinks it drags the skin on the opposite face with it. The common mistake is to check the rib thickness and forget the intersection, which is where the extra mass actually is.

The result is a shallow dimple, often only hundredths of a millimetre deep.

On a textured matte surface you won't see it. On a glossy black cosmetic face, especially under a window light, you'll see it from across the room.

Ribs: the most common cause I find

The rule of thumb for ribs is a thickness of 50 to 60% of the nominal wall for low-shrink amorphous materials, and 40 to 50% for high-shrink ones like PP or nylon. On a 2.5 mm ABS wall that's a 1.25 to 1.5 mm rib. On the same wall in PP, closer to 1 to 1.25 mm. Glass-filled grades shrink differently along and across the flow, so check the datasheet rather than the generic family figure.

Designers break this constantly, and I understand why. A thin rib looks flimsy in CAD and it's tempting to make it match the wall "for strength". But one full-thickness rib won't give you stiffness that two thinner, slightly taller ones can't, and it will sink. Stiffness comes from height, not thickness.

The root fillet matters as much as the rib. A radius of 0.25 to 0.5 times the wall reduces stress concentration, but a big generous fillet adds mass exactly where you don't want it. I'd rather see two thin ribs with small fillets than one thick rib with a lovely big one.

(Draft adds thickness too. A 15 mm tall rib with 1 degree per side is about 0.5 mm thicker at the root than at the tip, so check the root dimension, not the number on the sketch.)

Bosses, thick spots and the parts nobody cored out

Screw bosses sink for the same reason: a solid cylinder joined to the wall. The fix is to core them out and tie them in with thin ribs or gussets rather than merging them straight into the wall. A boss wall around 60% of nominal is a reasonable start, and if the boss sits right behind a cosmetic face I'll usually suggest moving it, or standing it slightly off the wall on a short connecting rib so the mass isn't directly under the surface.

Thick spots are sneakier. A part designed as a block and then shelled usually ends up uniform, but parts that grew feature by feature often have lumps: a 5 mm mounting flange on a 2 mm housing, a solid handle, a logo embossed on the inside face. Run a thickness analysis. Fusion 360 can colour every area above, say, 1.3 times nominal, and that map alone finds most of the problems.

If you're working in a material with a wide shrink range, such as a glass-filled nylon, I'd also ask the molder for their shrink figure before finalising boss positions, because the spacing between two bosses 150 mm apart can move by more than a millimetre between a 0.5% and a 1.2% assumption.

A few months ago I reviewed a small electronics housing where the only predicted sink was on the front face, right over a solid 6 mm mounting lug on the inside. Coring the lug into a U-shape with a 1.5 mm wall cost nothing in function and removed the thick mass. That's the typical case: ten minutes of CAD now, or weeks of process tweaking later.

Process fixes, and why I don't rely on them

The molder can reduce sink with more hold pressure, a longer hold time, a cooler mold on the cosmetic side, or a gate moved closer to the thick area. A gate that freezes off before the thick section is packed is a classic cause, so gate size and location matter as much as the geometry. Mold temperature on the moving half matters too, because ribs usually sit on the core side. Ask what the molder plans to run before you assume anything.

All of these work to a degree. But they cost cycle time, they can add stress, flash or warpage, and they narrow the process window, so the part drifts out again when the material lot or the machine changes. A part that only looks good at the edge of its window will look bad on some ordinary Tuesday.

Can't change the geometry? Then hide it. A textured finish, even a light one, hides a lot. So does a deliberate design line or a small step on the outer surface right where the rib lands, which turns an accidental dimple into an intended feature. Gas assist and chemical foaming agents are options too, but they're tooling and material decisions with their own cost, and I'd only reach for them on genuinely thick parts.

What I'd actually check before the tool is quoted

  • Nominal wall: uniform within about 25%?
  • Every rib: thickness ratio to its wall, for this specific material.
  • Every boss: cored, tied in with ribs, not under a cosmetic face if avoidable.
  • Thickness map: anything over 1.3 times nominal needs a reason or a change.
  • Cosmetic faces: marked on the drawing, with gloss or texture stated.
  • Gate: where it is relative to the thickest area.

Marking cosmetic faces is the step teams skip, and it's the cheapest one. The molder can't prioritise what nobody told them matters. If a little sink on the inside of a battery cover is fine, say so, and nobody wastes effort chasing it.

I keep a wider list in the DFM checklist, and the page on injection molding DFM questions covers what a molder will ask before quoting. If you'd like a second pair of eyes on one specific part, my injection molding DFM review looks at exactly these points.

The first review is free.

You can request a free initial DFM review here, and we'll agree an NDA before you share any CAD.

Questions people ask

How deep does a sink mark have to be before you can see it?

It depends on the surface. On a high-gloss dark part, a few hundredths of a millimetre can show under raking light, while a textured matte surface hides several times that. That's why cosmetic faces should be marked on the drawing with their finish.

Does a thicker wall reduce sink marks?

Usually the opposite. Thicker walls hold heat longer and shrink more, so they tend to sink more and add cycle time. A uniform wall of the right thickness for the material behaves better than a thick one.

Can sink marks be fixed after the mold is made?

Partly. The molder can adjust hold pressure, hold time, temperatures and sometimes gate size. Removing steel to thin a rib is also possible, and it's cheaper than adding steel. Texturing the cavity is another fix after the fact.

What is the difference between sink marks and voids?

Both come from the same shrinkage. If the skin is soft enough it gets pulled in and you get a sink mark. If the skin is already rigid, the core shrinks away from it inside the part and leaves a void. Fixing the thick section fixes both.

Want a second pair of eyes on your part?

The first DFM review of one part or assembly is free: short written manufacturability notes, no simulation, no redesign. We sign an NDA first if the CAD is confidential.

Request a free initial review

More from the blog